Mitsubishi Power Americas will add 450,000 square feet and more than 220 jobs at Savannah Machinery Works in Georgia as demand for advanced-class gas turbines grows.
This article finds that comprehensive root cause failure analysis are neccasery to provide different methods to alleviate the cause of stress corrosion cracking.